Packing for Flue Gas Desulfurization (FGD)
FGD scrubbers contact hot, corrosive flue gas carrying SO₂, SO₃, chlorides and fly ash with an alkaline slurry. Packing must resist acid attack, resist fouling from gypsum and fly ash, and maintain low pressure drop so the induced-draft fan energy stays low. A wrong material choice leads to rapid corrosion, plugging, or excessive energy cost.
The Operating Environment
Saturated acidic slurry, chlorides present, abrasive fly ash, temperatures typically 50–70°C, slurry with gypsum and limestone particles.
Packing Selection Logic
Corrosion resistance is the first filter: PP or PVDF for the wet zone, with PVDF preferred where chlorides or higher temperature exist. Open geometry resists plugging by gypsum and fly ash, so large-surface, high-void packing is preferred. Pressure drop must stay low to limit fan power. The efficiency–capacity–pressure-drop triangle favours larger nominal sizes with generous void fraction.
Recommended Products
| Product | Why It Fits |
| Plastic Pall Ring (PP/PVDF) | Open geometry resists plugging; PP or PVDF resists the acidic, chloride-bearing slurry. |
| Tri-Pack | High drip points and void fraction give good gas-liquid contact without trapping solids. |
| Vane Mist Eliminator | Downstream demisting removes entrained slurry droplets without plugging, unlike mesh pads. |
Common Failure Modes & How to Avoid Them
- PP used where chlorides or temperature exceed its limit — leads to embrittlement and collapse.
- Mesh demisters plugging with gypsum and fly ash, raising pressure drop and flooding.
- Fine packing (small nominal size) trapping slurry solids and blinding the bed.
- Underestimated liquid load causing channeling and poor SO₂ removal.
Frequently Asked Questions
Which material is best for FGD packing?
PP for the standard wet zone, PVDF where chlorides are significant or temperature is higher. Metal is rarely used in the wet FGD zone due to acid attack.
How do I prevent gypsum from plugging the packing?
Choose open, high-void geometry with a larger nominal size, ensure adequate liquid irrigation, and avoid dead zones. Tri-Pack and large pall rings resist solids accumulation.
What pressure drop should I design for?
Keep packing pressure drop low to control fan energy. We size packing to your gas rate to stay within your pressure budget.
Should the demister be mesh or vane type?
Vane type. Mesh pads plug rapidly with gypsum and fly ash; vanes tolerate solids and can be washed.
Can I retrofit existing FGD packing?
Yes, we supply replacement packing matched to your tower dimensions and can advise on upgrading to higher-void geometry.
Related Packing & Internals
Plastic pall ring in PP, PVDF and PTFE for corrosive and low-temperature scrubbing. Lightweight, chemical-resi…
Tri-Pack spherical random packing for scrubbers and strippers. High surface area, low pressure drop, excellent…
Vane-type chevron mist eliminator for high gas velocity and high liquid load. Handles fouling. Factory-direct …
Wire mesh demister pad / mist eliminator for separating entrained liquid droplets from gas streams. Factory-di…
Get a recommendation for Packing for Flue Gas Desulfurization (FGD)
Tell us your flow rate, medium and operating conditions — we recommend the right packing and internals, and quote factory-direct.
Request a Quote WhatsApp